Direct visualization of initial SEI morphology and growth kinetics during lithium deposition by in situ electrochemical transmission electron microscopy

Chem Commun (Camb). 2014 Feb 28;50(17):2104-7. doi: 10.1039/c3cc49029g. Epub 2014 Jan 13.

Abstract

Deposition of Li is a major safety concern existing in Li-ion secondary batteries. Here we perform the first in situ high spatial resolution measurement coupled with real-time quantitative electrochemistry to characterize SEI formation on gold using a standard battery electrolyte. We demonstrate that a dendritic SEI forms prior to Li deposition and that it remains on the surface after Li electrodissolution.